Hello folks,
We have a project where the customer had a problem with ants getting into
and onto the circuit assembly mounted in a box, on a wall on the outside of
a house.
The Conformal coating material was able to provide all the protection they
required - formic acid - and was based upon a single component polyurethane
coating applied by means of dipping.
I have a complete article and photo's provided by the customer which I will
be happy to share with those interested, if you would please contact me off
line.
Regards, Graham Naisbitt
[log in to unmask]
Concoat Ltd Phone: +44 1276 691100
Alasan House Fax: +44 1276 691227
Albany Park
CAMBERLEY
GU15 2PL UK
Any opinions expressed are those of this employer.
-----Original Message-----
From: Bernard Williams <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: 10 September 1998 23:47
Subject: [TN] Environmental testing - insects
>Clive:
>Yep, sounds strange but I came across the term on a PCB testing facility's
>web pages (as part of a series of tests on populated PCB boards). (They
didn't reply to my email)
>
>In any case we are concerned with ants/cockroaches blowing up our
>high voltage IGBT dpak devices and am looking for anyone with
experience/solutions.
>Termites in NZ aren't that big or hungry!
>
>We have a great example where an ant has been forever immortalised
>when climbing up this dpak device. It used the gate lead as a step for one
foot and that centre drain "stub" as a step for another foot. It's frozen
dead (not vapourised) and so is the device!
>Seems enough charge went through the ant to raise the gate voltage and put
the IGBT
>into its linear region with consequent overheating and failure.
>
>Potting would be a solution but it is expensive.
>Conformal coat doesn't really work, it isn't very rugged,
>especially over sharp points.
>
>Perhaps noone really worries too much about this sort of thing but if
>anyone has experience in this area it would be great to hear from you.
>
>Bernard Williams
>(Electronic Engineer)
>_________________________________
>Fisher & Paykel
>Laundry Division
>78 Springs Rd., East Tamaki, Auckland.
>PO Box 58-732, Greenmount, Auckland.
>
>Tel: (09) 273-0640 ext.6695.
>Fax: (09) 273-0649
>Email: [log in to unmask]
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|