Inform your customer that a contract for soldering to MIL-STD 2000 is
uninforceable.
The closing of the Goverment Schools rendered MIL-STD 2000 Task G impossible
to achieve. There is no Category certification available to meet the
requirements of the specification. Are they calling out MIL-STD 2000A whose
requirements can be met? They are actually very different documents and
have different lead tinning requirements.
Single point soldering is soldering one termination at a time.
I will fax you Mil-STD 2000 Par. 4.11.3 , par. 5.4.4, and par 5.4.17.6
Al Cash
> ----------
> From: Rick Thompson[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Rick Thompson
> Sent: Thursday, August 27, 1998 4:43 PM
> To: [log in to unmask]
> Subject: [TN] MIL-2000 Lead Tinning?
>
> Hi,
>
> We have a customer who is requesting a quote to build PCBAs with a
> requirement for lead tinning & 'single-point' soldering per Mil-2000. He
> knows that Mil-2000 has been superceded but their customer is still
> requiring it. I don't have a copy of Mil-2000 and was wondering if
> someone
> could briefly tell me what the lead tinning requirements of the spec were,
> was it a requirement at all times or only when solderability testing
> failed,
> etc. Also, what the term 'single-point' soldering refers to; I'm not
> familiar with the term.
>
> Thanks.
>
> Rick Thompson
> Ventura Electronics Assembly
> 2665A Park Center Dr.
> Simi Valley, CA 93065
>
> [log in to unmask]
>
> (805) 584-9858 voice
> (805) 584-1529 fax
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|