Hello Fellow Technetters.
I have little experience with thru-hole technology assemblies, as we build
mainly double sided SMT.
The question I have is:
Can SO8 /14/16/20 devices be passed thru the wave solder (on the
solder side of the PWB) without solder defects such as bridging? I have
read about "solder thieves" but have no details.
Does anyone have experience with wave soldering SMDs that they could
pass along any advice?
Thanks in advance,
Ernst Wallisch
Manufacturing Ops.
Computing Devices Canada
[log in to unmask]
(613) 596-7536
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|