The Dynaloy Co. is in Indianapolis Indiana. Phone # 800-669-5790
There is a complete line of URESOLVE products in addition to DYNASOLVE.
The URESOLVE's are based on methanol or ethylene glycol ether
chemistries depending on what type of coating and substrate you are
working with. Their applications people should be able to direct you to
the correct product when supplied with the materials of construction you
are dealing with.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett Wa.
425-356-6076
On Tue, 5 May 1998 09:47:53 -0700 RSIMathis wrote:
> From: RSIMathis <[log in to unmask]>
> Date: Tue, 5 May 1998 09:47:53 -0700
> Subject: [TN] Uresolve Plus
> To: [log in to unmask]
>
> Hi, everyone.
>
> I'm looking for a chemical (solvent ?) called Uresolve or Uresolve Pls made by
> a company named Dynalloy. (I'm not sure about this name?) This stuff is used
> for dissolving conformalcooatings and potting compounds. Does anyone have any
> information where to purchase this substance OR how to contact this company?
> OR any info about a similar substance?
>
> What I'm trying to do is dissolve the plastic overmolding on a custom cable
> assembly to check out the internal construction. I'm open to any and all
> suggestions. Thanks for the help.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|