The Dynaloy Co. is in Indianapolis Indiana. Phone # 800-669-5790 There is a complete line of URESOLVE products in addition to DYNASOLVE. The URESOLVE's are based on methanol or ethylene glycol ether chemistries depending on what type of coating and substrate you are working with. Their applications people should be able to direct you to the correct product when supplied with the materials of construction you are dealing with. Regards Michael Barmuta Staff Engineer Fluke Corp. Everett Wa. 425-356-6076 On Tue, 5 May 1998 09:47:53 -0700 RSIMathis wrote: > From: RSIMathis <[log in to unmask]> > Date: Tue, 5 May 1998 09:47:53 -0700 > Subject: [TN] Uresolve Plus > To: [log in to unmask] > > Hi, everyone. > > I'm looking for a chemical (solvent ?) called Uresolve or Uresolve Pls made by > a company named Dynalloy. (I'm not sure about this name?) This stuff is used > for dissolving conformalcooatings and potting compounds. Does anyone have any > information where to purchase this substance OR how to contact this company? > OR any info about a similar substance? > > What I'm trying to do is dissolve the plastic overmolding on a custom cable > assembly to check out the internal construction. I'm open to any and all > suggestions. Thanks for the help. > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################