Jan,
I can't answer you for the first question.
For the second question, (even though I don't have the same
wavesoldering machine as you have) it is obvious to me that the
solder pot needs some serious maintenance and good
cleaning.
When a heavy layer of dross gets build-up in the pot, the pump
action of motor pulls down bits of dross under molten solder and
pumps up thru wave nozzles. Crusty layers of dross build up on
solder pot steel walls, and restrict or block solder flow. The
pumping mechanical action grinds dross into fine powder and
push them thru the wave. The first thing I suggest to do is
remove and clean the pumping mechanism. If it still causes
dross thru the wave, remove solder as much as you. And
remove plates and nozzles and give good scrubbings to remove
crusty layers of dross from metal surfaces.
re.
Matthew Park
NII-Norsat International Inc.
>>> "<Jan Satterfield>" <[log in to unmask]> April 6,
1998 2:53 pm >>>
Can anyone help my coworker on a dross problem?
>----------
>From: Mallory, Michael @ SLC
>Sent: Thursday, April 02, 1998 9:22 AM
>To: Satterfield, Jan @ SLC
>Subject: Smartwave Floss Paper
>
>Jan, will you send a question (s) off to technet in regards to
"Floss" paper
>for the spindle on the smart wave of a Soltec Deltawave
6622CC wave soldering
>machine. The question's are; Is there another place to
purchase this high
>temp paper and if so who, what is the part number. Has
anyone else
>experienced the problem of dross using this type of machine?
The dross
>appears to be coming out through the smartwave. Let me
know if you need more
>info.
>
>Thanks
>Mike
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|