I have very little experience, but I have only seen Kirkendall voiding
mentioned with regard to the wire bonding process (typically the
gold-aluminum interfaces). From a wire bonding perspective, wouldn't
increasing the temperature or dwell time increase the possibility of
voiding since diffusion rates usually increase with increasing temperature?
George Harman has a few pages on Kirkendall Voiding in his "Wire Bonding in
Microelectronics..." book, but I don't know if you can apply the
information to soldering.
Hopefully someone else will have a better answer.
Dave Anderson
Medtronic, Inc.
Opinions are my own, and not necessarily those of my employer.
>>> "Yuen, Mike" <[log in to unmask]> 03/16/98 03:08pm >>>
As I know it, Kirkendall voiding is caused by rapid diffusion of gold
molecules. It was typically related to gold finishes. My question is:
What else can be done to reduce the formation of such void other than
reduce gold thickness?
How about increase dwell time at reflow soldering?
Regards
MIchael Yuen
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|