Rudy Shubert at Bellcore did considerable published work, ca. late
1980's early 1990's, on fretting corrosion of Au/Au (the best),
Au/Sn (the worst) and Sn/Sn (pretty good) contacts. I have the
reference somewhere, but I'd have to dig pretty deep to retrieve it.
I don't know if this is a particular problem with SIMM's, but it
can lead to high contact resistances with pcb finger contacts
in high-vibration environments, and hence electrical unreliability.
----------
> From: Lee McCuistion <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] Mating Tin / Gold; SIMMs and sockets
> Date: Tuesday, February 24, 1998 5:01 AM
>
> Ok,
> Who has some technical details, study, or white paper on the validity
> of, or problems with mating tinned fingered SIMMs with gold contact
> sockets or visa-versa? Does this really have any effect on
> reliability?
>
> Lee McCuistion
> Manufacturing Engineer
> Cubix Corporation
> 2800 Lockheed Way
> Carson City, NV 89706
> 702-888-1000 x237 (voice)
> 702-888-1002 (fax)
> [log in to unmask] (e-mail)
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|