Karen,
I could not agree more. Currently one of our major headaches is the
issue of PCB cleanliness from our suppliers. Using a solution (75% DI /
25 % IPA) heated to 140 F and a spray cycle of 15 minutes, we have
some PCB Manufacturers supplying product at <2 ug / sq in , several in
the range of 15 - 20 ug / sq in and some in the range of 25-35 ug / sq in.
The middle group causes us many hassles, and the latter is simply
intolerable. The fact that we get product at <2 shows that it can be done
if the suppliers WANTS to. As long as tap water is the wash medium
and the cleanliness testing is the cold, < 4 minute test you mentioned,
they might as well be doing no testing at all and stop wasting their time.
>>> Karen Tellefsen <[log in to unmask]> 01/24/98 12:12pm
>>>
Mark Simmons wrote:
> Some of the advantages to HAL are:
> 1. Solderability. Nothing solders like solder.
Absolutely, probably HASL best advantage.
> With respect to Cleanliness, <3 mg. cl. sq. in. is routine on modern
> equipment.
You'd probably get < 3 mg Cl/in^2 even if you clean in ice cold tap
water for 5 seconds. (m = milli)
However, 3 micrograms Cl/inch^2 on HASLed boards, while do-able with
modern PC fab equipment, is hardly routine except for the best
fabricators. That is unless one measures ionic contamination with an
unheated Omegameter with a test time < 4 min as is done by many PC
fab shops. A lot of HASLed boards are pretty dirty, ionically speaking.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|