TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
JON MOORE <[log in to unmask]>
Date:
Mon, 26 Jan 1998 10:33:05 -0500
Content-Type:
text/plain
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, JON MOORE <[log in to unmask]>
Parts/Attachments:
text/plain (59 lines)
Karen,
   I could not agree more.   Currently one of our major headaches is the
issue of PCB cleanliness from our suppliers.  Using a solution (75% DI /
25 % IPA) heated to 140 F and a spray cycle of 15 minutes, we have
some PCB Manufacturers supplying product at <2 ug / sq in , several in
the range of 15 - 20 ug / sq in and some in the range of 25-35 ug / sq in.
The middle group causes us many hassles, and the latter is simply
intolerable.  The fact that we get product at <2 shows that it can be done
if the suppliers WANTS to.  As long as tap water is the wash medium
and the cleanliness testing is the cold, < 4 minute test you mentioned,
they might as well be doing no testing at all and stop wasting their time.

>>> Karen Tellefsen <[log in to unmask]> 01/24/98 12:12pm
>>>
Mark Simmons wrote:
> Some of the advantages to HAL are:
> 1.  Solderability.  Nothing solders like solder.

Absolutely, probably HASL best advantage.

> With respect to Cleanliness, <3 mg. cl. sq. in. is routine on modern
> equipment.

You'd probably get < 3 mg Cl/in^2 even if you clean in ice cold tap
water for 5 seconds.  (m = milli)

However, 3 micrograms Cl/inch^2 on HASLed boards, while do-able with
modern PC fab equipment, is hardly routine except for the best
fabricators.  That is unless one measures ionic contamination with an
unheated Omegameter with a test time < 4 min as is done by many PC
fab shops.  A lot of HASLed boards are pretty dirty, ionically speaking.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2