TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Mon, 19 Jan 1998 11:54:22 EST
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Engelmaier <[log in to unmask]>
Content-type:
text/plain; charset=ISO-8859-1
Subject:
From:
Engelmaier <[log in to unmask]>
Organization:
AOL (http://www.aol.com)
Content-transfer-encoding:
quoted-printable
Parts/Attachments:
text/plain (64 lines)
Hi Larry,
There has been an IPC sponsored study, in which non-functional (dead) pads
were a part. The results are reported in IPC-TR-579, “Round Robin Reliability
Evaluation of Small Diameter Plated Through Holes in Printed Wiring Boards,”
where Conclusion 23 reads: "Functional and nonfunctional innerlayer lands
appear to improve reliability" with the effect so small that no recommendation
is made regarding the use of non-functional lands.
In a previous TechNet discussion on this subject, I submitted:
"This has been a long ongoing debate. 
The work done for IPC-TR-579, 'Round Robin Reliability Evaluation of Small
Diameter Plated Through Holes in Printed Wiring Boards', indicated a small
improvement in reliability with the presence od functional and non-functional
innerlayer lands. This was NOT a major finding of this study, nor was it a
recommendation for the use of non-functional innerlayer lands. 
The results of the just released ITRI Report, 'PWB Hole-to-Land
Miregistration: Causes and Reliability', give the same indication (Note:
essentially all the failures come from one PWB manufacturer, primarily from
PTV barrel cracking, before the test was stopped at about 1100 cycles; the
other manufacturers show some interconnect separations of the innerlayer trace
from the barrel). The 1997 ITRI report also shows the vast improvement in the
quality of PTV structures since the 1988 IPC-TR-579 study. 
The ITRI study was done with temperature cycling from -65<->+125C; thus, the
reliability results directly, on an accelerated basis, relate to the thermal
cycling PWBs see in product operation. However, because no excursions were
taken to soldering temperatures, where because of being above Tg of the epoxy
significantly more thermal expansion mismatch occurs and the epoxy is much
softer, the results can not be assumed to be representative of what might
happen during PWB assembly. It is during solder temperature excursions that
the compressive hydro-static hoop stresses act on the PTV barrel and that
surface and innerlayer land rotations occur. These represent quite different
loading conditions than -65<->+125C temperature cycling, and may produce
different conclusions.
CONCLUSIONS: Non-functional lands are not likely worth having, because the
small potential reliability gain for high-reliability PTV structures for most
applications in not worth the manufacturing difficulties and costs that have
been encountered. Misregistration and the absence of annular rings are no
significant reliability threat to PTV barrels. Assuming, that the behavior
during solder temperature excursions is not dramatically different and the PTV
interconnect structure survives assembly, misregistration and the absence of
annular rings are no significant reliability threat to PTV interconnects
(Interconnects can be protected from large loads by having a 90 degree trace
jog just before the PTV, i.e. do not approach the PTV with a long straight
trace)."

Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]


##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################

ATOM RSS1 RSS2