TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Mon, 5 Jan 1998 12:48:32 EST
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Engelmaier <[log in to unmask]>
Content-type:
text/plain; charset=ISO-8859-1
Subject:
From:
Engelmaier <[log in to unmask]>
Organization:
AOL (http://www.aol.com)
Content-transfer-encoding:
quoted-printable
Parts/Attachments:
text/plain (40 lines)
Hi Paul,
I was the chairman of the committee that produced IPC-SM-785.
The high acceleration isothermal mechanical cycling referred to on page 7 can
be performed at either room or elevated temperatures. The test referred to is
the one developed for the IEEE Compliant Lead Task Force in the 1983
timeframe. Essentially all the testing was performed on a test apparatus
conceptualised by the Task Force leaning on an initial DEC-design, the
detailed design was done by AMP, which also build the first 20 test machines
for the Task Force. This test apparatus is available from Anatech, 6
Whittemore Terrace, Wakefield, MA  01880-2252, 617-245-7825,
[[log in to unmask]]. Ask for John Sofia. Anatech also build Event
Detectors, that allow you to properly monitor for failures. I cna mention the
supplier, since to my knowledge nobody else builds anything comparable. IBM
also developed a high acceleration isothermal mechanical cycling
technique—this one uses PWB twisting instead of PWB bending—which they
commercially sell as well. However, I can for the moment not lay my fingers on
the appropriate contact information—I just relocated, and my files are still a
mess. I do not get any commisions from either company, by the way. 

Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]


##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2