TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 12 Jan 1998 22:09:03 EST
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, RSedlak <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Organization:
AOL (http://www.aol.com)
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (22 lines)
This is a chronic problem when you put OSP, or in general microetch,  a board
that also has gold plating, as on tips.   I do not know anybody who has solved
it, except in the extreme case of taping, or otherwise covering the gold,
before you go into microetch.

Good luck

Rudy Sedlak
RD Chemical Company

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2