This is a chronic problem when you put OSP, or in general microetch, a board that also has gold plating, as on tips. I do not know anybody who has solved it, except in the extreme case of taping, or otherwise covering the gold, before you go into microetch. Good luck Rudy Sedlak RD Chemical Company ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################