Mr. Yee, the results are not extraordinary. It has been observed before.
Sometimes at high humidity, a sort of cleaning takes place due to the
micro washing actions of the water molecules. So a cleaner surface will
show high resistance. If you leave it long enough, degradation of
resistance will show up. Hope it helps.
##############################################################