I have a question about some SIR results that I got. I made a few
consecutive SIR tests on a coupon and found that the ohm reading kept
on increasing the longer I left the coupon inside the humidity chamber
(35C, 85%RH). My understanding is that the reading should normally
decrease with the elapsed time, indicating the lowering of surface
resistance, right? I ran the coupon for 1 week, at first the ohm
reading looked OK (~2-5e11 ohm), but at the end of the week the
reading esceeded 1e12 ohm. I am confused.
T.G.Yee
Hadco Kuching
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|