TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Paul Klasek <[log in to unmask]>
Date:
Mon, 5 Jan 1998 17:44:40 +1100
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Paul Klasek <[log in to unmask]>
Parts/Attachments:
text/plain (83 lines)
Hi Kevin , & ALL
To cut the esoteric pad area, gold slip layers calculations etc. short :
In practice when you actually get to do it, it's simple :
If you rip the pad off you're home , if you don't you have something to
worry about .
I did try small joints, BIG joints (PS) ; it applies reliably .
Therefore despite the theoretical complexity of all theoretical factors
( pad area, oxide-vetability, gold layers slip, plating, etc.) you CAN
make life easier on yourself just by making it a simple polarised
dilemma , which it in a fact is .
I started the same way before realised that for the trees I could not
see the forest .

So for the sheer adhesion by all means do establish the fact the pad
gave up , than you have a piece of mind ,
unless you need better than that . Than it's a different game
(substrate)

For High acceleration isothermal mechanical cycling , at elevated level
temperature ;
read for some hints page 7 , IPC-SM-785 , Guidelines for accelerated rel
. test ........  ,
the info is limited to stating what is it and that it exists somewhere
in the IPC files .
We need an IPC fellow to shed a light on this option of quick fix test
of limited but useful data acquisition .
I could be only guessing that it does consist of board flex cycling at ?
temperature .
There must be somebody who knows, otherwise it would not be noted in 785
.

See you
             Paul  (ResMed)

>----------
>From:  Engelmaier[SMTP:[log in to unmask]]
>Sent:  Saturday, 3 January 1998 1:10
>To:    [log in to unmask]
>Subject:       Re: [TN] pull test std
>
>Hi Kelvin,
>To my knowledge, there is no standard on pull testing leads or shear testing
>chip components, nor should or could there be. First, the high variability in
>pad/lead/component desig gives you too many variables; second, the pull/shear
>strength per se does not give you an indication of the solder joint
>reliability. Observation of the fracture surfaces can, however, give you
>information whether or not your solder joints are properly wetted.
>
>Werner Engelmaier
>Engelmaier Associates, L.C.
>Electronic Packaging, Interconnection and Reliability Consulting
>7 Jasmine Run
>Ormond Beach, FL  32174  USA
>Phone: 904-437-8747, Fax: 904-437-8737
>E-mail: [log in to unmask]
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2