TECHNET Archives

December 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Date:
Fri, 5 Dec 1997 13:39:16 -0800
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (21 lines)
     Marcello:

     Yes, each thermal cycle will remove a small portion of the ENTEK-106A.
     However, ENTEK-106A will withstand 6-8 thermal cycles before it is
     sufficiently degraded to be of concern (and that is typically at 200+
     degrees C.).  In addition, the first thermal cycle actually makes it
     more chemically resistant.

     Since the typical process flow is either single reflow (1 cycle), dual
     reflow (2 cycles), single reflow with wave solder (2 cycles) or single
     reflow with Glue + wave solder (3 cycles), there is more than enough
     margin for a bake after ENTEK application.  Right?

     Bill Fabry