Rolled Solder is a method used to coat single sided boards with
solder..it involves a solder pot and a transfer roller that applys
solder to the boards as they pass over the roller...
Prior to hot air leveling it was the method used in place of tin/lead
plate and reflow....It allowed a conveyorized method of solder
application which low cost single sided boards needed to stay
competitive...
Doug Jeffery...
You wrote:
>
>This is a multi-part message in MIME format.
>--------------608D52B1BA7F1F6A1F509FED
>Content-Type: text/plain; charset=us-ascii
>Content-Type: text/plain; charset=us-ascii
>Content-Transfer-Encoding: 7bit
>Content-Transfer-Encoding: 7bit
>
>Technetters,
>
> Could anyone shed some light ont the term "rolled
>solder" finish on pwb's? I have had a couple of people ask me about
it
>and am curious to find out more. Any comments would be appreciated.
>Thanks .
>
>CHET.
>
>--------------608D52B1BA7F1F6A1F509FED
>Content-Type: text/x-vcard; charset=us-ascii; name="vcard.vcf"
>Content-Transfer-Encoding: 7bit
>Content-Description: Card for Chetan Mehta
>Content-Disposition: attachment; filename="vcard.vcf"
>
>begin: vcard
>fn: Chetan Mehta
>n: Mehta;Chetan
>org: Eagle Circuits
>adr: 10820 Sanden Drive;;;Dallas;Texas;75238;
>email;internet: [log in to unmask]
>tel;work: 214 349-0288
>tel;fax: 214 349-1210
>x-mozilla-cpt: ;0
>x-mozilla-html: FALSE
>end: vcard
>
>
>--------------608D52B1BA7F1F6A1F509FED--
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|