Rolled Solder is a method used to coat single sided boards with solder..it involves a solder pot and a transfer roller that applys solder to the boards as they pass over the roller... Prior to hot air leveling it was the method used in place of tin/lead plate and reflow....It allowed a conveyorized method of solder application which low cost single sided boards needed to stay competitive... Doug Jeffery... You wrote: > >This is a multi-part message in MIME format. >--------------608D52B1BA7F1F6A1F509FED >Content-Type: text/plain; charset=us-ascii >Content-Type: text/plain; charset=us-ascii >Content-Transfer-Encoding: 7bit >Content-Transfer-Encoding: 7bit > >Technetters, > > Could anyone shed some light ont the term "rolled >solder" finish on pwb's? I have had a couple of people ask me about it >and am curious to find out more. Any comments would be appreciated. >Thanks . > >CHET. > >--------------608D52B1BA7F1F6A1F509FED >Content-Type: text/x-vcard; charset=us-ascii; name="vcard.vcf" >Content-Transfer-Encoding: 7bit >Content-Description: Card for Chetan Mehta >Content-Disposition: attachment; filename="vcard.vcf" > >begin: vcard >fn: Chetan Mehta >n: Mehta;Chetan >org: Eagle Circuits >adr: 10820 Sanden Drive;;;Dallas;Texas;75238; >email;internet: [log in to unmask] >tel;work: 214 349-0288 >tel;fax: 214 349-1210 >x-mozilla-cpt: ;0 >x-mozilla-html: FALSE >end: vcard > > >--------------608D52B1BA7F1F6A1F509FED-- > >############################################################## >TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c >############################################################## >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TECHNET <your full name> >To unsubscribe: SIGNOFF TECHNET >############################################################## >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. >For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 >############################################################## > ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################