Currently I am trying to evaluate Lea Ronal Actronal for acid descaler
for alloy42 .
Any comments . I am quite a bit worried due to the sulphuric acid based
.Furthermore
we have a short length of the line exposed to air which I believe could
contribute
to the yellowish brown smut and causing adhesion problem .Please reply asap.
At 02:18 PM 10/30/97 UT, you wrote:
> With regard to the inquiry on Alloy 42 pre-treatment below, most
companies
>who are plating this base material today use proprietary cleaning/descaling
>processes which have been designed for specific lead frame alloys, Alloy 42
>included. These processes are available from a number of suppliers, LeaRonal
>included, but as Technet is not a commercial forum, I will not go into the
>specifics of our process. In general, all of these types of pre-treatment
>processes contain one or more oxidizing agents, acid (usually sulfuric), and
>possibly other compounds such as inhibitors or mild chelating agents. Finding
>the right combination of ingredients to properly pre-treat the material
>without causing problems in the plating process is what the specialty chemical
>suppliers are supposed to do.
>
> If you've not had success with other products and if you desire more
>information you can contact me off-line.
>
> Rob Schetty
> LeaRonal Inc.
>(T) 516-868-8800
>(F) 516-867-5917
>
>----------
>From: TechNet on behalf of tonghh
>Sent: Thursday, October 30, 1997 7:22 AM
>To: [log in to unmask]
>Subject: [TN] Alloy42
>
> Hello to all technetters :
>
> Recently I have been trying to figure out the best pretreatment method for
> alloy42 materials for further plating processes .Could someone share some
> info on this , since alloy42 materials is very sensitive in nature . We
> have tried using 5% sulphuric acid and others proprietary chemicals also
> sulphuric acid based , the operating window is limited .
>
> Thanks .
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|