TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Date:
Fri, 31 Oct 1997 22:21:13 +0800
Content-Type:
text/plain; charset="us-ascii"
X-To:
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, tonghh <[log in to unmask]>
Parts/Attachments:
text/plain (47 lines)
At 11:43 AM 10/30/97 -0500, you wrote:
>Our customers have found that a good alkaline cleaner, used as hot as
>possible, and as long as possible, perhaps even used as an electrocleaner, to
>shorten the process time, is the key, after that any weak acid solution,
>Sulfuric is great, then rinse and plate.
>
>I can give you more information directly, or contact Dynavest, or their
>subsidiary Comacraft, with offices in Penang, KL, Manilla, and Singapore.
>
>Rudy Sedlak
>RD Chemical Company
   To : Rudy sedlak

    Thanks a lot for your input .I have tried that before but it do not work .
    Please elaborate further on sulphuric acid , operating % , temperature , any
    ppm of Fe or Ni the bath can tolerate because sulphuric acid will attack
alloy42
    and gives rise to Fe3+ and a yellowish brown discoloration to the alloy42 .
    Please advise .Thanks .
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2