Charles Barker@IO-US Wrote
10/20/97 11:31 AM
>The QQ-S-571E spec shows a .0050% max acceptable level of Zinc in the
>alloy, but I couldn't find anything referencing Cobalt in this spec.
Acceptable contaminants level could also have slight variation upon the
actual ratio of Sn to Pb in the alloy.
##############################################################