Hi Charles,
Thanks for the information. Who is the sponsoring organization of the spec.
you mentioned (QQ-S-571E)? Where can I get a copy?
Rob Schetty
LeaRonal Inc.
----------
From: TechNet on behalf of Charles Barker
Sent: Monday, October 20, 1997 12:31 PM
To: [log in to unmask]
Subject: Re: [TECHNET] Assembly
Charles Barker@IO-US
10/20/97 11:31 AM
The QQ-S-571E spec shows a .0050% max acceptable level of Zinc in the
alloy, but I couldn't find anything referencing Cobalt in this spec.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|