TECHNET Archives

September 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
TechNet Mail Forum<[log in to unmask]>
Subject:
From:
"CSS Asia Co., Ltd." <[log in to unmask]>
Date:
Tue, 2 Sep 1997 20:42:12 +0900
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, "CSS Asia Co., Ltd." <[log in to unmask]>
Parts/Attachments:
text/plain (21 lines)
Hi Technetters.

One of the largest flexible PCB shop in Korea tried to laminate PI coverlay
of one mil thick  onto one mil/one ounce RA PI flexibles and floated  them
on a solder pot at 300 degree C for ten second.  All the test coupons
blistered.  They claimed that Japanese coverlay withstands such condition,
and asked us to improve the thermal resistance of the coverlay.    I would
like to be advised of your opinion on the test and its validity in real
field.  In other word,  what do you see out of the 300 C test?   Could you
give me some light to lead persuade them into 288 C test ?