Rick --

Great question! I wish the industry as a whole would standardize on this! I 
would be very interested in hearing what other replies you get back.

We count defects basically the same way you do,  but with some variations 
depending on the defects were tracking: 

Solder defect rate:

	# of defective solder joints / total # of solder joints

Placement defect rate or defective component defect rate:
	# of defective placements or defective components / total # of 
components

Total process-related defect rate:

	(# of defective solder joints + # of placement defects) / (total # of 
solder joints + total # of components)

Over-all defect rate:
	(# of defective solder joints + # of placement defects + # of defective 
components) / (total # of solder joints + 2*(# of components))

 Since the "over-all" defect rate includes electrically defective components, 
each component has an additional opportunity to be defective.   

# of defective solder joints = the number of pins affected. If one whole side of 
a 60-pin QFP is shorted together, that's 15 defective solder joints.

 The exception is that if just two pins are shorted together, I suspect this 
just gets counted as 1 defect most of the time.

If the QFP is misclocked, that's one defective placement.

If the QFP has an internal defect, that's one defective component.


-- Vickie Chapman

 


On Wed, 9 Jul 1997 10:33:41 -0700 RICK VERNON wrote:

> From: RICK VERNON <[log in to unmask]>
> Date: Wed, 9 Jul 1997 10:33:41 -0700
> Subject: PPM Defect Counting
> To: [log in to unmask]
> 
> We count our defect opportunities as follows: one per component plus
> one per solder joint. A resistor would be three defect opportunities, a 144
> pin QFP would be 145 defect opportunities.
> 
> We count actual defects as follows: Tombstone part is one defect.
> Insufficient solder on one pad is one defect. Solder short between three
> legs of an SOIC is one defect. Skewed SOIC is one defect.
> 
> I have concerns that we are presenting an artificially low PPM rate by
> counting defects this way. Others have concern that if we count defects
> the same way we create opportunities, the PPM numbers will be inflated.
> 
> I'm looking for info on how others in the industry count actual defects that
> affect more than one opportunity.
> 
> Thanks.  Rick Vernon, QA Manager   [log in to unmask]
> 
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
> * with <subject: subscribe/unsubscribe> and no text in the body.          *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact   *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
> ***************************************************************************
> 



***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2