Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wtzNk-000BkKC; Thu, 31 Jul 97 12:51 CDT |
Content-Type: |
text/plain; charset=US-ASCII |
Old-Return-Path: |
|
Date: |
Thu, 31 Jul 1997 13:00:53 -0500 |
Precedence: |
list |
Resent-From: |
|
Message-ID: |
|
>From willli Thu Jul 31 12: |
51:46 1997 |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Mime-Version: |
1.0 |
Content-Description: |
cc:Mail note part |
Subject: |
|
From: |
|
From [log in to unmask] Thu Jul 31 12: |
59:17 1997 |
Resent-Message-ID: |
<"706hI2.0.kXM.R2Dup"@ipc> |
Content-Transfer-Encoding: |
7bit |
Resent-Sender: |
|
Parts/Attachments: |
|
|
I remember that years ago there was a process called printed through holes that
essentially printed conductive material through a hole to make a double sided
board. This technology may not be used anymore, being replaced by plated through
holes. This did nearly fill holes.
______________________________ Reply Separator _________________________________
Subject: Fab/Assy: Thermal Vias
Author: [log in to unmask] at INTERNET
Date: 7/31/97 8:24 AM
Hello Technetters,
Has anyone found a method to completely fill a via? I don't think
that the standard plating process will guarantee 100 % fill. We're also
looking at the option of screen printing conductive epoxy and trying to force
it through the hole. But, I don't have a lot of confidence in this process
either. The last option we're considering would be to plug the vias with LPI
soldermask. This seems like the best guarantee of fill. Thermal conductivity
is not so great, but it is better than air.
I'd sure appreciate any comments.
Glenn Pelkey
Quality/Reliability Engineer
Maxtek Components Corp.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|