I remember that years ago there was a process called printed through holes that essentially printed conductive material through a hole to make a double sided board. This technology may not be used anymore, being replaced by plated through holes. This did nearly fill holes. ______________________________ Reply Separator _________________________________ Subject: Fab/Assy: Thermal Vias Author: [log in to unmask] at INTERNET Date: 7/31/97 8:24 AM Hello Technetters, Has anyone found a method to completely fill a via? I don't think that the standard plating process will guarantee 100 % fill. We're also looking at the option of screen printing conductive epoxy and trying to force it through the hole. But, I don't have a lot of confidence in this process either. The last option we're considering would be to plug the vias with LPI soldermask. This seems like the best guarantee of fill. Thermal conductivity is not so great, but it is better than air. I'd sure appreciate any comments. Glenn Pelkey Quality/Reliability Engineer Maxtek Components Corp. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************