TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wmJKW-000BjgC; Thu, 10 Jul 97 08:32 CDT
Content-Type:
text/plain; charset=us-ascii
Old-Return-Path:
Date:
Thu, 10 Jul 1997 07:41:14 -0700
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/13893
From [log in to unmask] Thu Jul 10 08:
51:03 1997
TO:
Return-Path:
<TechNet-request>
X-Status:
X-Loop:
Resent-Message-ID:
<"UIt0t3.0.X-9.ZHEnp"@ipc>
>From willli Thu Jul 10 08:
32:35 1997
Subject:
From:
[log in to unmask] (Sam Pirayesh)
Content-Transfer-Encoding:
7bit
Message-ID:
Organization:
S00
X-Mailer:
Mozilla 2.02 (Win16; I)
Parts/Attachments:
text/plain (22 lines)
Hi All,
Recently I heard of Solderability issue and lead fracture on fine picth QFP (16 mils or 
less) during vabiration test on the PWB with Electroless Nickle and Immersion 
Gold finish (100u-200u of Nickle and 3u-5u of gold) , couple reason was mention one 
being the flux used during the assembly and another was the Nickle passivation on the 
PWB before assembly. 
Is any of you have any experience with this problem and if you do, what you have done to 
correct the problem. Also I am interested on all the good things you can tell me about 
this finish type.
Thanks.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2