TECHNET Archives

May 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Wed, 21 May 1997 10:00:00 -0400 (EDT)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
From [log in to unmask] Wed May 21 10:
51:29 1997
Status:
O
>From bergdi Wed May 21 08:
50:52 1997
X-Sender:
TO:
Return-Path:
<TechNet-request>
X-Status:
X-Loop:
Resent-Message-ID:
<"-KhJx.0.78A.cslWp"@ipc>
Subject:
From:
Sheila Smith <[log in to unmask]>
X-Mailing-List:
<[log in to unmask]> archive/latest/12859
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wUBmh-000Bj1C; Wed, 21 May 97 08:50 CDT
X-Mailer:
Windows Eudora Pro Version 2.1.2
Message-Id:
Parts/Attachments:
text/plain (34 lines)
>Date: Wed, 21 May 1997 09:46:43
>To: [log in to unmask]
>From: Sheila Smith <[log in to unmask]>
>Subject: RE:  Copper sulphide corrosion
>
>John,
>
>I assume you have confirmed the presence of copper sulphide by chemical
analysis, not just by appearance or color?  If the silicone is an acetoxy
curing RTV, it could be releasing corrosive byproducts during the cure--
that is generally common knowledge in the industry so most folks wouldn't
use that type of cure system silicone but you probably should ask the
question of your supplier.
>
>We don't typically use a silicone for this type of application -- adhesion
is too much of a problem.  We use a urethane or epoxy conformal coating or,
if additional thermal conductivity or mechanical strength  is needed, we use
a filled, flexibilized epoxy.  Feel free to email me directly if you'd like
more details.
>
>Sheila Smith, TRACOR AES
>

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2