Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset="us-ascii" |
Old-Return-Path: |
|
Date: |
Wed, 21 May 1997 14:07:16 -0700 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
From [log in to unmask] Wed May 21 10: |
50:33 1997 |
Status: |
O |
X-Mailing-List: |
|
X-Sender: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
>From bergdi Wed May 21 07: |
57:09 1997 |
X-Status: |
|
Resent-Message-ID: |
<"F8_Fd1.0.nX6.I4lWp"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wUAwm-000Bj1C; Wed, 21 May 97 07:56 CDT |
X-Mailer: |
Windows Eudora Pro Version 2.2 (16) |
Message-Id: |
|
Parts/Attachments: |
|
|
Hi
We have seen failures on a bought-in assembly due to growth of copper
sulphide on the copper traces of a flexible PCB. The failure occurs at the
base of SnPb solder joints, where the copper traces are not covered by
photoresist. The whole area of exposed copper and solder joints is covered
by a silicone based potting material.
Unfortunately our supplier is not being very helpful, so I am looking for
clues as to what is happening and how to stop it myself.
The source of sulphur is not known, but there are various rubber components
within the immediate area.
Does anyone have any experience of this type of corrosion system? If so, I
would appreciate a discussion about the factors involved - in particular,
the role of the potting compound and whether an alternative passivating
material would do a better job.
Thank you
John Loveluck
Group Quality Manager
Tadpole Technology plc
Cambridge Science Park
Cambridge CB4 4RB
Tel: (+44)1223.428200
Fax: (+44)1223.428201
email: [log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|