TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
TEXT/PLAIN; CHARSET=US-ASCII
From [log in to unmask] Tue Mar 18 12:
40:05 1997
Old-Return-Path:
Date:
Tue, 18 Mar 97 18:28:23 PST
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11162
TO:
Return-Path:
<TechNet-request>
X-Loop:
Resent-Message-ID:
<"79gvG.0.9fJ.MwiBp"@ipc>
Subject:
X-Priority:
3 (Normal)
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w72Xg-000BBnC; Tue, 18 Mar 97 11:19 CST
From:
X-Mailer:
Chameleon 4.6, TCP/IP for Windows, NetManage Inc.
Message-Id:
Parts/Attachments:
TEXT/PLAIN (30 lines)
Dear collegues ,


We are developping a designrulebook for design for manufacturing of
Au Thin Wire Wedge/Wedge  and Ribbon Bonding especially for High Frequency 
Applications.

Is there anyone,  who knows  designrules for DFM for  similar or  other 
wire/ribbon bond applications  coming from the Chip on board technology. May be that there still exists a structure for such a Designrulebook.

I think it makes sense to work together in a userforum  on this matter.

Is  there anyone  who is interested in this matter ?

Thank You very much

M. Jeremias

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2