We are currently looking into alternatives to HASL on our PWB's. Our
boards contain
primarily fine pitch surface mount parts with some thru-hole. The
alternatives I have seen are
OPC (Entek Plus CU-106A), Nickel/Gold, and Electroless Palladium. In all
of the data
the I have gathered on alternatives, I have yet to see a comparison between
the alternatives.
Does anyone have any data comparing the various alternatives or personal
experience? I
would appreciate any input that you may have. Thank you.
Best Regards,
Mike Forrester
Sr. Test Engineer
LeCroy Corp.
E-Mail: [log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|