I agree. With proper placement and restraints, it is more representative of what you want to measure. Isn't that what it is all about?
John Guy
American Competitiveness Institute (EMPF)
317-655-3673 x130
[log in to unmask]
----------
From: Bob Willis[SMTP:[log in to unmask]]
Sent: Friday, January 10, 1997 10:53 AM
To: INTERNET:[log in to unmask]
Subject: Re: ASSY: thermocouple adhesive
Why not use solder its better !
Bob Willis
Process Engineering Consultant
Electronic Presentation Services
2 Fourth Avenue, Chelmsford, Essex CM1 4HA. England.
Tel: (44) 01245 351502
Fax: (44) 01245 496123
Home Page: http://ourworld.compuserve.com/homepages/Bwillis
Email: [log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|