TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Thu, 16 Jan 1997 08:30:26 -0800 (PST)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9302
From [log in to unmask] Thu Jan 16 15:
11:21 1997
TO:
Return-Path:
<TechNet-request>
X-Loop:
Resent-Message-ID:
<"X2FZu2.0.gPG.HFcto"@ipc>
Subject:
From:
Bob Mesick <[log in to unmask]>
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vkvWG-0000TWC; Thu, 16 Jan 97 11:22 CST
X-Sender:
X-Mailer:
Windows Eudora Light Version 1.5.2
Message-Id:
Parts/Attachments:
text/plain (24 lines)
Just a quickie,

The local 1 hour photo shops here in california use resin columns to reclaim
the silver.  The developer is just passed throught the columns to drain.
The silver is recovered by a service.  A plateout cell probably will not get
you down to EPA silver limits but resin will.

Bob Mesick
Remco Engineering (remco.com/home.htm)
Industrial Water and Wastewater Treatment Systems
San Luis Obispo, California  USA

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2