'CAF' stands for Conductive Anodic Filament and it is basically the term used
for the formation of a conductive pass, usually along a glass fiber, that leads
to a failure.
Tom Carroll
Hughes Aircraft Company
_______________________________________________________________________________
Subject: Acronyms
From: [log in to unmask] at CCGATE
Date: 4/2/96 5:46 AM
Bring me up to speed here. What does CAF stand for? As used here talking
about the polyamide failures topic of the week,
"This failure sounds like the "CAF" failure studied by Bell Labs in the late
70's and early 80's."
====================================================================
George Franck
PWB Product Assurance Phone (703) 560-5000 x2648
E-Systems M/S N408 Fax (703) 280-4613
7700 Arlington Blvd E-Mail: [log in to unmask]
Falls Church Va 22046 E-Mail: [log in to unmask]
====================================================================
The following is an attached File item from cc:Mail. It contains
information that had to be encoded to ensure successful transmission
through various mail systems. To decode the file use the UUDECODE
program.
--------------------------------- Cut Here ---------------------------------
begin 644 rfc822.txt
M4F5C96EV960Z(&)Y(&-C;6%I;"!F<F]M(&5D96XN:&%C+F-O;0T*1G)O;2!4
M96-H3F5T+7)E<75E<W1`:7!C+F]R9PT*6"U%;G9E;&]P92U&<F]M.B!496-H
M3F5T+7)E<75E<W1`:7!C+F]R9PT*4F5C96EV960Z(&9R;VT@<VEM;VXN:7!C
M+F]R9R`H,38X+C$Q,RXR-"XV-"D-"B!B>2!%1$5.+DA!0RY#3TT@*%!-1$8@
M5C0N,RTW(",U.#@T*2!I9"`\,#%),S(P,$HR2S8X,#`P54%-0$5$14XN2$%#
M+D-/33X[(%1U92P-"B`R($%P<B`Q.3DV(#`U.C0U.C,S(%!35`T*4F5C96EV
M960Z(&9R;VT@:7!C+F]R9R!B>2!S:6UO;BYI<&,N;W)G('9I82!33510("@Y
M-#`X,38N4T=)+C@N-BXY+SDT,#0P-BY31TDI#0H@:60@2$%!,C(S,C$[(%1U
M92P@,B!!<'(@,3DY-B`P-SHT-CHR-2`M,#@P,`T*4F5C96EV960Z(&)Y(&EP
M8RYO<F<@*%-M86EL,RXQ+C(X+C$@(S(I(&ED(&TP=30V,E0M,#`P,#9:0SL@
M5'5E+`T*(#(@07!R(#DV(#`W.C(R($-35`T*4F5S96YT+61A=&4Z(%1U92P@
M,#(@07!R(#$Y.38@,#<Z-#8Z,C4@+3`X,#`-"D1A=&4Z(%1U92P@,#(@07!R
M(#$Y.38@,#@Z,S`Z,30@+3`U,#`-"E)E<V5N="UF<F]M.B!496-H3F5T0&EP
M8RYO<F<-"D9R;VTZ(&=F<F%N8VM`;65L<&%R+F5S>7,N8V]M("A'96]R9V4@
M1G)A;F-K("!8,C8T."[log in to unmask]"D-"E-U8FIE8W0Z($%C<F]N>6US#0I297-E
M;G0M<V5N9&5R.B!496-H3F5T+7)E<75E<W1`:7!C+F]R9PT*4F5S96YT+7-E
M;F1E<CH@5&5C:$YE="UR97%U97-T0&EP8RYO<F<-"E@M4V5N9&5R.B!G96]R
M9V5`,3$N,"XP+C<R#0I4;SH@=&5C:&YE=$!I<&,N;W)G#0I297-E;G0M;65S
M<V%G92UI9#H@/")30VUS9C(N,"YJ-D8N1F5)3VXB0&EP8SX-"DUE<W-A9V4M
M:60Z(#QV,#$U,3`Q,#1A9#@V9&(P961A,31`6S$Q+C$X+C$N.%T^#0I-24U%
M+79E<G-I;VXZ(#$N,`T*0V]N=&5N="UT>7!E.B!T97AT+W!L86EN.R!C:&%R
M<V5T/2)U<RUA<V-I:2(-"D-O;G1E;G0M=')A;G-F97(M96YC;V1I;F<Z(#="
M250-"D]L9"U2971U<FXM4&%T:#H@/&=F<F%N8VM`;65L<&%R+F5S>7,N8V]M
M/@T*6"U-86EL:6YG+4QI<W0Z(#Q496-H3F5T0&EP8RYO<F<^(&%R8VAI=F4O
M;&%T97-T+S,R-3<-"E@M3&]O<#H@5&5C:$YE=$!I<&,N;W)G#0I0<F5C961E
+;F-E.B!L:7-T#0H`
end
|