George, 'CAF' stands for Conductive Anodic Filament and it is basically the term used for the formation of a conductive pass, usually along a glass fiber, that leads to a failure. Tom Carroll Hughes Aircraft Company _______________________________________________________________________________ Subject: Acronyms From: [log in to unmask] at CCGATE Date: 4/2/96 5:46 AM Bring me up to speed here. What does CAF stand for? As used here talking about the polyamide failures topic of the week, "This failure sounds like the "CAF" failure studied by Bell Labs in the late 70's and early 80's." ==================================================================== George Franck PWB Product Assurance Phone (703) 560-5000 x2648 E-Systems M/S N408 Fax (703) 280-4613 7700 Arlington Blvd E-Mail: [log in to unmask] Falls Church Va 22046 E-Mail: [log in to unmask] ==================================================================== The following is an attached File item from cc:Mail. It contains information that had to be encoded to ensure successful transmission through various mail systems. To decode the file use the UUDECODE program. --------------------------------- Cut Here --------------------------------- begin 644 rfc822.txt M4F5C96EV960Z(&)Y(&-C;6%I;"!F<F]M(&5D96XN:&%C+F-O;0T*1G)O;2!4 M96-H3F5T+7)E<75E<W1`:7!C+F]R9PT*6"U%;G9E;&]P92U&<F]M.B!496-H M3F5T+7)E<75E<W1`:7!C+F]R9PT*4F5C96EV960Z(&9R;VT@<VEM;VXN:7!C M+F]R9R`H,38X+C$Q,RXR-"XV-"D-"B!B>2!%1$5.+DA!0RY#3TT@*%!-1$8@ M5C0N,RTW(",U.#@T*2!I9"`\,#%),S(P,$HR2S8X,#`P54%-0$5$14XN2$%# M+D-/33X[(%1U92P-"B`R($%P<B`Q.3DV(#`U.C0U.C,S(%!35`T*4F5C96EV M960Z(&9R;VT@:7!C+F]R9R!B>2!S:6UO;BYI<&,N;W)G('9I82!33510("@Y M-#`X,38N4T=)+C@N-BXY+SDT,#0P-BY31TDI#0H@:60@2$%!,C(S,C$[(%1U M92P@,B!!<'(@,3DY-B`P-SHT-CHR-2`M,#@P,`T*4F5C96EV960Z(&)Y(&EP M8RYO<F<@*%-M86EL,RXQ+C(X+C$@(S(I(&ED(&TP=30V,E0M,#`P,#9:0SL@ M5'5E+`T*(#(@07!R(#DV(#`W.C(R($-35`T*4F5S96YT+61A=&4Z(%1U92P@ M,#(@07!R(#$Y.38@,#<Z-#8Z,C4@+3`X,#`-"D1A=&4Z(%1U92P@,#(@07!R M(#$Y.38@,#@Z,S`Z,30@+3`U,#`-"E)E<V5N="UF<F]M.B!496-H3F5T0&EP M8RYO<F<-"D9R;VTZ(&=F<F%N8VM`;65L<&%R+F5S>7,N8V]M("A'96]R9V4@ M1G)A;F-K("!8,C8T."[log in to unmask]"D-"E-U8FIE8W0Z($%C<F]N>6US#0I297-E M;G0M<V5N9&5R.B!496-H3F5T+7)E<75E<W1`:7!C+F]R9PT*4F5S96YT+7-E M;F1E<CH@5&5C:$YE="UR97%U97-T0&EP8RYO<F<-"E@M4V5N9&5R.B!G96]R M9V5`,3$N,"XP+C<R#0I4;SH@=&5C:&YE=$!I<&,N;W)G#0I297-E;G0M;65S M<V%G92UI9#H@/")30VUS9C(N,"YJ-D8N1F5)3VXB0&EP8SX-"DUE<W-A9V4M M:60Z(#QV,#$U,3`Q,#1A9#@V9&(P961A,31`6S$Q+C$X+C$N.%T^#0I-24U% M+79E<G-I;VXZ(#$N,`T*0V]N=&5N="UT>7!E.B!T97AT+W!L86EN.R!C:&%R M<V5T/2)U<RUA<V-I:2(-"D-O;G1E;G0M=')A;G-F97(M96YC;V1I;F<Z(#=" M250-"D]L9"U2971U<FXM4&%T:#H@/&=F<F%N8VM`;65L<&%R+F5S>7,N8V]M M/@T*6"U-86EL:6YG+4QI<W0Z(#Q496-H3F5T0&EP8RYO<F<^(&%R8VAI=F4O M;&%T97-T+S,R-3<-"E@M3&]O<#H@5&5C:$YE=$!I<&,N;W)G#0I0<F5C961E +;F-E.B!L:7-T#0H` end