Good morning:
I guess I've never heard that particular jargon for it, but we
used to see it, particularly on Duroid-type materials, with the
impingement of the jets in a jet pumice scrubber and later with the
aluminum oxide jet scrubber. It's a good argument for having a chem
clean optional cleaning process, if you can stand the redundancy.
Marc Carter
|
|
|