Dear Lee,
why do you need lower phosperous content ? to process boards at lower temp
than what is recommended by chemistry supplier.
Nickel has crystalline structure at low phosphorus content (upto 3 to 4 % P)
hence gets tarnished /oxidises very easily. If you use low phosphorus EN, then you may need an activator between EN and IG which often may not work satisfactorily.Result gold peeloff if you do tape test.
Normally the chemistry supply EN for ENIG finish with P content between
8 to 10 % . also while operating the bath the phosphorus content varies depending on PH and reducer.
normally we bake boards at 140 C to check for tarnishing of Gold. The gold
does not tarnish if you put sufficient gold and it works.
radhakrishnan
indal eletronics
india
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|