Subject: | |
From: | |
Date: | 14 Nov 1996 15:19:07 -0700 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Grade FR-6: polyester resin, glass mat reinforced. Suggest you
contact some of the laminate manufacturers about availability.
Floyd Gentry
Sandia National Labs
______________________________ Reply Separator _________________________________
Subject: FR6 Laminate
Author: [log in to unmask] at hubsmtp
Date: 11/14/96 4:24 AM
Does anyone out there know what FR6 is, and who supplies it ?