Steve: Try Aremco Products Inc.(914)762-0685.They make a variety of
electrically conductive adhesives that use Ag,Ni or C depending on
the amount of conductivity required.They have epoxy systems that will
go to 320 C intermittent and ceramic ones that will go to over 600 C.
Good Luck!
Regards
Michael Barmuta
Fluke Corp.
Everett Wa.
(206)356-6076
On Thu, 14 Nov 1996 14:21:37 -0800 [log in to unmask] wrote:
> From: [log in to unmask]> Date: Thu, 14 Nov 1996 14:21:37 -0800
> Subject: Elec. Cond. Adhesive for Hi Temp
> To: [log in to unmask]
>
> Is there an electrically conductive adhesive which will survive a reflow
> at 220-240 C while maintaining reasonable bond strength? Probably not,
> but I thought I'd ask anyway.
>
>
> [log in to unmask]
> ph:503-359-9300 ext. 54653
>
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To unsubscribe from this list at any time, send a message to: *
> * [log in to unmask] with <subject: unsubscribe> and no text. *
> ***************************************************************************
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|