Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vW3c0-0000YoC; Fri, 6 Dec 96 10:58 CST |
Content-Type: |
TEXT/PLAIN; charset=US-ASCII |
Old-Return-Path: |
|
From [log in to unmask] Fri Dec 6 15: |
32:20 1996 |
Precedence: |
list |
Resent-From: |
|
cc: |
|
MIME-Version: |
1.0 |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
X-Loop: |
|
Resent-Message-ID: |
<"hpRh22.0.g1O.F35go"@ipc> |
Subject: |
|
From: |
|
Message-ID: |
<Pine.3.89.9612060933.A12862-0100000@netcom17> |
In-Reply-To: |
|
Resent-Sender: |
|
Date: |
Fri, 6 Dec 1996 09:03:33 -0800 (PST) |
Parts/Attachments: |
|
|
Mostly glass bodied, some not. They are glued, nothing special per
say, other than close attention to profile in the preheat/wave. To tell
you the truth, we've seen far more problem with ceramic caps than the
diodes.
Stew Benedict
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|