Mostly glass bodied, some not. They are glued, nothing special per say, other than close attention to profile in the preheat/wave. To tell you the truth, we've seen far more problem with ceramic caps than the diodes. Stew Benedict *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************