Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vDtLe-0000RMC; Thu, 17 Oct 96 09:22 CDT |
From [log in to unmask] Thu Oct 17 12: |
05:03 1996 |
Date: |
Thu, 17 Oct 1996 10:23:19 -0400 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"tKSTW3.0.uAI.e4aPo"@ipc> |
Subject: |
|
From: |
|
Old-Return-Path: |
|
X-Loop: |
|
Message-ID: |
|
Parts/Attachments: |
|
|
STELLA,
YOU MAY WANT TO TRY REDUCING THE APERTURE SIZE ON YOUR STENCIL.
I WOULD SUGGEST A 2 MIL ANULAR REDUCTION WOULD PROBABLY BE ENOUGH.YOU MAY
ALSO WANT TO INCREASE YOUR SQUEEGEE PRESSURE A LITTLE TO TRY TO REDUCE THE
AMOUNT OF BLEED OUT AROND THE PAD,AND ALSO REDUCE THE THE AMOUNT OF PASTE
LEFT ON THE BOTTOM OF THE STENCIL AFTER EACH PRINT CYCLE.
PAUL
EC TRONICS , NJ
***************************************************************************