STELLA, YOU MAY WANT TO TRY REDUCING THE APERTURE SIZE ON YOUR STENCIL. I WOULD SUGGEST A 2 MIL ANULAR REDUCTION WOULD PROBABLY BE ENOUGH.YOU MAY ALSO WANT TO INCREASE YOUR SQUEEGEE PRESSURE A LITTLE TO TRY TO REDUCE THE AMOUNT OF BLEED OUT AROND THE PAD,AND ALSO REDUCE THE THE AMOUNT OF PASTE LEFT ON THE BOTTOM OF THE STENCIL AFTER EACH PRINT CYCLE. PAUL EC TRONICS , NJ *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************