Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0v3YTz-0000SZC; Wed, 18 Sep 96 21:04 CDT |
Old-Return-Path: |
|
Date: |
Wed, 18 Sep 1996 22:13:21 -0400 |
Precedence: |
list |
Resent-From: |
|
From [log in to unmask] Thu Sep 19 10: |
22:02 1996 |
Message-ID: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"WliQ81.0.kv9.1fAGo"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Resent-Sender: |
|
Parts/Attachments: |
|
|
In a message dated 96-09-18 11:42:26 EDT, you write:
> And another:where does the lead carbonate come ?
>
>
Lead oxidizes to Lead Oxide, or Lead Hydroxide, (Lead Hydroxide = Lead Oxide
+ Water) then reacts with either Carbon Dioxide in the air (suspect less
likely) or with Carbonates in water (suspect more likely) and Bingo!
***************************************************************************