Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0v3RDb-0000SyC; Wed, 18 Sep 96 13:19 CDT |
Encoding: |
60 Text |
Old-Return-Path: |
|
Date: |
Wed, 18 Sep 96 13:22:31 cst |
Precedence: |
list |
Resent-From: |
|
Cc: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"3N_gw3.0.CIJ.jq3Go"@ipc> |
Subject: |
|
From [log in to unmask] Wed Sep 18 14: |
50:39 1996 |
X-Loop: |
|
Resent-Sender: |
|
From: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Hi Phil:
I have two references that talk about the solderability and pumice
scrub interactions:
"Thwaites, C.J. and Mackay, C.A., "Some Effects of Abrasive Cleaning
on the Solderability of Printed Circuits", Metal Finishing Journal,
Sept. 1968, pp. 291-294 (Tin Research Institute Publication 386).
"Spiliotis, N.J., "Tin Lead Plating Practices That Assure Proper
Wetting Upon Reflow", Insulation/Circuits, June 1978, pp. 64-71."
I imagine that Paul Davis used the Thwaites/Mackay efforts for at least part of
a publication - I can't find any record of a paper by him on pumice scrubbing
but then my library has a few holes in it. As for your dewetting and white
residue question - NO, I have run into that situation several times but it was
never a lead species related issue. Tin preferentially oxidizes on a tin/lead
surface which makes the formation of a lead species a process specific cause. Do
the pwbs see some type of chemistry and/or environmental exposure that would
promote a lead carbonate? I think Bill Hampshire (formerly of the Tin Research
Institute) published a paper that talked about the formation of lead species -
you may want to get ahold of him (I know I have the paper but I just can't find
it!).
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: Dewetting & Pumice Scrub
Author: [log in to unmask] at ccmgw1
Date: 9/18/96 10:41 AM
Technetters
In the mid 1970's Paul Davis of Tin Research wrote an article on dewetting as
result of pumice scrub. Does anyone have a reference to where this was
published. Also does anyone have any input as to dewetting as result of pumice
scrub in relation to a sequence of: (1) pumice scrub, (2)apply solder mask, (3)
hot air level, (4)solderability test and dewet..
Another question on dewetting. Has anybody seen dewetting as a result of a
white residue on the lands and board which was analyzed as lead carbonate?
And another:where does the lead carbonate come ?
Phil Hinton
Hinton PWB Engineering
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|