Jim  at Motorola asked:

Does anyone know where to clean some populated printed wiring boards using
supercritical carbon dioxide (CO2)?  
..........................................................reply..................
...........................

Try Dr Sean Adams at AIRCO/BOC,  he is usually up to speed on on matters
involving gases if he can't help directly. Don't know if he has EMAIL,  but fax
is 908 771 1709