We have not placed any BGAs yet.  I understand that another advantage is
that if the vias are the correct diameter, they can aid in manual placement
(ie: the solder balls drop into the via barrels very slightly.

-Pat-

-------------
Patrick McGuine
Nicolet Instrument
[log in to unmask]
(608) 276-6334