Subject: | |
From: | |
Date: | Thu, 27 Jul 95 16:36:40 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
If this is referring to press fit connector holes, our vendor
tolerances are +/- .001 on the copper plating and +/- .002 on the
solder plating. We have had problems in the past with Board
Manufactures exceeding these tolerances and the Press Fit connectors
are very hard to install.
If not "Never Mind"
ERic Bernal
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: Press fit padstacks
Author: [log in to unmask] at ~INTERNET
Date: 7/27/95 3:03 PM
Received: by ccmail
Received: from netcomsv by pragma.com (UUPC/extended 1.11) with UUCP;
Thu, 27 Jul 1995 15:02:33 PDT
Received: from miso.wwa.com by netcomsv.netcom.com with SMTP (8.6.12/SMI-4.1)
id OAA10881; Thu, 27 Jul 1995 14:32:22 -0700
Resent-Date: Thu, 27 Jul 1995 14:32:22 -0700
Received: from ipc by miso.wwa.com with uucp
(Smail3.1.28.1 #8) id m0sbaZB-000FRDC; Thu, 27 Jul 95 16:34 CDT
Received: by ipchq.com (Smail3.1.28.1 #2)
id m0sbZyV-0000GsC; Thu, 27 Jul 95 15:56 CDT
Old-Return-Path: <miso!starman.convex.com!ondricek>
Date: Thu, 27 Jul 95 15:44:57 -0500
From: [log in to unmask] (Doug Ondricek)
X-ccAdmin: postmaster@netcomsv
Message-Id: <[log in to unmask]>
To: [log in to unmask]
Subject: Press fit padstacks
Resent-Message-ID: <"x23x-1.0.e16.Zr_5m"@ipc>
Resent-From: [log in to unmask]
X-ccAdmin: postmaster@netcomsv
X-Mailing-List: <[log in to unmask]> archive/latest/752
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]
I'd like to get some feedback on what other people are using for pad and
antipad sizes relative to finished hole size on press fit holes.
Thanks in advance,
Doug Ondricek
Convex Computer Corporation
Ph: (214) 497-4794
Fax:(214) 497-4441
email: [log in to unmask]
|
|
|